Views: 0 Author: Site Editor Publish Time: 2022-05-31 Origin: Site
Are you suffering from the high return rate of products? Do you often receive complaints about the black surface peeling or fading of the black faucet?
Let me introduce to you, why does black surface peel so easily? There are three kinds of black plating processes in the market.
1. Painting black: The advantage of this surface treatment is that the cost is very low. But its shortcomings are also obvious, especially easy to fall off the whole piece. You can take a look at the following image, which shows the faucet matte black surface peeling from the tube.
2. Electron painting: This electroplating process is the most common. This kind of electroplating has strong adhesion, not easy to peel off. However, if the connection of a product is often collided, it is easy to fade. For example, the shower handset often take out and put it back to the shower holder, In this case, the shower is easy to fade.
3. Oxidized black: This black treatment is oxidized and blackened on the surface of acid copper. This black surface treatment process performs well in all aspects. The only disadvantage is that the cost is a little high.
Landonbathstarted to produce black faucets when black became popular, at the beginning, we made the black faucet with Paint black, delivery to the first client, they sold to the market, Then there were many complaints to the client for the black surface peeling everyday, after that they never order from us, we lost that client for ever.
After this incident, we found that the black spray paint could not be used on the high end faucet at all. We were looking for a better black plating, we used electroplated black, Most customers are very satisfied with this surface, But soon we received complaints from some famouse brand customers about this surface treatment, peeling occurs at the connection or detail of the products. They need us to handle all the details well. Then we went to seek a more better black plating process.
We started testing oxidized black, Continuously collided and insert at the connection, It was found that there was no peeling at the two connections. Since then, we have not received any complaints about black surface treatment.
If you are still suffering from the black peeling off, You can try our oxidized black.